How is iridium extracted by wet method?

1. Alkali fusion separation: Mix the material evenly with a certain proportion of sodium hydroxide and sodium peroxide, and calcine at 800°C for 8-12 hours. After cooling, take it out and break it into pieces. Use water to leach the…

Platinum chloride separation process

Platinum chloride separation process

Platinum chloride separation process 1, Basic principle. After the dissolution of platinum chloride oxidation, add ammonium chloride to sink platinum, filter the sunken platinum residue after roasting to get crude platinum, crude platinum after chlorination and oxalic acid in addition…